#Paintinginspector #coatingdefects
Abrasion, Adhesion Failure, Alligatoring (Crocodiling), Bleeding, Blistering, Bloom (Blush), Bridging, Bubbles or Bubbling, Cathodic Disbonding, Chalking, Checking, Cissing, Cobwebbing, Cracking, Cratering, Crazing, Crowsfooting, Delamination, Fading, Flaking, Grinning, Heat Damage, Impact Damage, Intercoat Contamination, Mud Cracking, Orange Peeling, Peeling, Pinholes, Rippled Coating, Runs, Rust Rashing, Rust Spotting, Rust Staining, Sags, Settlement, Skinning, Solvent Lifting, Solvent Popping, Staining, Stress Cracking, Undercutting, Wrinkling,
Please subscribe and support.
0:00 Introduction
0:06 ABRASION
0:34 ADHESION FAILURE Probable Causes: Surface
0:56 Alligatoring (Crocodiling)
1:24 Bleeding
1:44 Blistering Blistering
2:17 Bloom (Blush) Bloom (Blush)
2:39 Bridging Bridging
2:55 Bubbles or Bubbling Bubbles or Bubbling
3:34 Cathodic Disbonding
4:01 Checking
4:48 Cobwebbing Cobwebbing
6:10 Crows footing Crowsfooting
6:30 Delamination Delamination
6:58 Flaking
7:41 Grinning Grinning
7:57 Heat Damage Heat Damage
8:10 Impact Damage Impact Damage
8:44 Mud Cracking Mud Cracking
9:04 Orange Peeling Orange Peeling
9:21 Peeling Peeling
9:35 Pinholes Pinholes
10:06 Rippled Coating Rippled Coating
10:43 Rust Rashing Rust Rashing
10:58 Rust Spotting Rust Spotting
11:35 Rust Staining Rust Staining
12:37 Skinning Skinning
12:56 Solvent Lifting Solvent Lifting
13:19 Solvent Popping Solvent Popping
13:35 Staining Staining
13:50 Stress Cracking
14:18 Undercutting Undercutting
14:43 Wrinkling Wrinkling